Abstract:
On the 30th anniversary of the Journal “Membrane Science and Technology”, it has also been about 30 years since ceramic membrane separation technology was employed for the civil purpose though it had served for long time in the concentration and separation of nuclear bomb fuels. This article would briefly recall its historical development; introduce the present status and prospect for the future in order to promote its key and innovative functions in the new industrial revolution.

Funds:

AuthorIntro:
孟广耀(1942年),男,山东省莱州人,主要研究方向:无机功能材料的固体化学与制备化学,长期从事陶瓷分离膜材料研制及其在工业与环境领域的技术应用,侧重新能源转换装置的开发。

Reference:
[1] 孟广耀, 周明, 彭定坤,多孔陶瓷膜制备、表征及其应用
薄膜科学与技术,  4(1991)54
[2] 周明, 孟广耀, 彭定坤等,Sol-gel 化学及新型无机材料
材料科学与工程,  9(3),8(1991)
[3] 熊国兴 古景华等,多组分金属氧化物膜的制备与表征,第一届全国膜与膜过程学术报告会文集,p439-443, 中国科学院主办,1991年10月,大连
[4] 孟广耀 彭定坤 编著:材料化学在中国科技大学:学科发展与研究实践,第4章,中国科技大学出版社,2011年5月,合肥
[5]  Zhou Ming, Meng Guangyao, peng Dingkun, Zhao Guien, Study on the Sol-gel process for TiO2 membrane formation, Key Eng. Mater. 61&62,11(1991), P.387
[6] Meng G.Y., Cao Ch. B, Yu W.J and Peng D.K,  Formation of ZrO2 and YSZ layers by microwave plasma assisted MOCVD,Key Eng. Mater. 61&62,11(1991)
[7] 孟广耀 第二届国际无机膜学术会议(ICIM2-91)情况介绍, 化学进展, Vol.6 (1991)
[8] 孟广耀 彭定坤 编著,“材料化学在中国科技大学:学科发展与研究实践”,第5章,中国科技大学出版社,2011年5月,合肥
[9] 王沛 邢卫红 徐南平 时钧等, 全国第二届膜与膜过程学术报告会论文集, 304-346页,共7篇论文,国家海洋局主办,1996年11月杭州。
[10] 孟广耀 彭定坤 编著,“材料化学在中国科技大学:学科发展与研究实践”,第6章,中国科技大学出版社,2011年5月,合肥
[11]王建红, 高铝多孔陶瓷支撑体的耐腐蚀性能研究,南京工业大学硕士论文, 2005
[12]李改叶,荣先辉, 一种韧性改善的Al2O3-YSZ支撑体制备与腐蚀性分析,解放军理工大学学报,10卷1期 (2009)67-70
[13]漆虹 邢卫红,范益群, “低温烧成高纯氧化铝陶瓷膜支撑体的制备“,
      硅酸盐学报 38卷2期(2010)283-293
[14]合肥长城新元膜科技公司网页:www.ccxym.cn
[15]张小珍,新型中空纤维陶瓷膜的制备科学与性能研究,
中国科技大学博士论文, 2011年6月
[16] 李健生, 郝艳霞, 王连军等, 氧化铝中空纤维膜的制备与表征[J]. \
催化学报,2001, 22 (5): 437-440.
[17] W. Yin, B. Meng, X. Meng, X. Tan,Highly asymmetric yttria stabilized zirconia hollow fibre membranes [J],J. Alloys Compd. 476 (2009) 566-570.
[18] 方大儒, 中空纤维陶瓷膜的制备研究,
中国科学技术大学硕士学位论文[D], 2009.
[19]任祥军,多孔陶瓷(膜)材料的研制及在气固分离中的应用研究,
中国科技大学硕士论文,2006
[20]李俊峰,林红,李建保等,高温过滤支撑体用SiC基多孔陶瓷的制备与表征, 稀有金属材料与工程,38卷2期,2009,122-125
[21] 中材科技股份有限公司网页 www.sinomatech.com
[22] .Yingchao Dong, Xingqin Liu, Qianli Ma, Guangyao Meng,
Preparation of cordierite-based porous ceramic micro-filtration membranes using waste fly ash as the main raw materials, Journal of Membrane Science, 285 (2006) 173-181.
[23]孟广耀 彭定坤, 无机膜-新的工业革命,
自然杂志, 第18卷3期,1996,151-156
[24]孟广耀,新能源体系与无机膜技术,膜科学与技术,29卷4期(2009)1-10
[25] X. Tan, Y. Liu, K. Li,Mixed conducting ceramic hollow-fiber membranes for air separation [J],AIChE Journal, 2005, 51(7): 1991-2000.
[26] Z.Wang, N. Yang, B. Meng, X. Tan, Preparation and oxygen permeation proper- ties of highly asymmetric La0.6Sr0.4Co0.2Fe0.8O3-x perovskite hollow-fiber membranes [J], Ind. Eng. Chem. Res. 2009, 48: 510-516.
[27] Z. Chen, R. Ran, Z. Shao, H.Yu, J.C. Diniz da Costa, S. Liu, Further performance improvement of Ba0.5Sr0.5Co0.8Fe0.2O3-δ perovskite membranes for air separation [J], Ceramics International 35 (2009) 2455-2461.
[28] 李伟,陶瓷中空纤维氧分离膜研究[D],
中国科学技术大学博士学位论文,2009.
[29] W. Li, T. Tian, F. Shi, Y. Wang, C. Chen, Ce0.8Sm0.2O3-δ-La0.8Sr0.2MnO3-δ Dual-Phase Composite Hollow Fiber Membrane for Oxygen Separation [J], Ind. Eng. Chem. Res. 2009, 48: 5789-5793.
[30] 杨春利Chunli Yang; Qiming Xu; Litao Yan; Wenping Sun; Zetian Tao; Wei Liu,Hydrogen permeation performance o 陶瓷中空纤维膜在气体分离和固体氧化物中的应用于研究f Ni-BaZr0.1Ce0.7Y0.2O3-δ metal-ceramic hollow fiber membrane, submitted(2,
中国科学技术大学 博士论文, 2010011)年 6月
[31] Chuli Yang, Wei Li, Shangquan Zhang, Lei Bi, Ranran Peng, Chusheng Chen, and Wei Liu, Fabrication and characterization of an anode-supported hallow fiber SOFC, J. Power Sources, 187 (2009)90-92
[32] Xiaozhen Zhanga,Bin Lin, Yihan Ling, Yingchao Donga, Guangyao Meng, Xingqin Liu, An anode-supported hollow fiber solid oxide fuel cell with (Pr0.5Nd0.5)0.7Sr0.3MnO3−?–YSZ composite cathode
Journal of Alloys and Compounds 497 (2010) 386–389
[33] 孟广耀,“陶瓷膜燃料电池研究进展与展望”,中国科学技术大学学报 第38卷(2008)576-593
 

Service:
Download】【Collect

《膜科学与技术》编辑部 Address: Bluestar building, 19 east beisanhuan road, chaoyang district, Beijing; 100029 Postal code; Telephone:010-80492417/010-80485372; Fax:010-80485372 ; Email:mkxyjs@163.com

京公网安备11011302000819号